First establish when a bridge forms near SMT copper hardware. Deposits joined immediately after printing require a different investigation from contours spreading during waiting or preheat. Preserve stage-specific evidence before changing paste, stencil, placement or queue conditions.

01

Locate the first change in contour

Indium distinguishes cold and hot slump and discusses rheology, deposit height and waiting conditions. Fraunhofer ISIT evaluates printed contour stability separately from wetting after melting. Deposits can merge before the solder melts.

We recommend numbered locations at minimum gaps, beneath copper hardware and beside nearby components. Record after printing, the planned maximum wait and approved preheat observation, noting sampling effects. If the initial print is already bridged, review apertures, alignment, release and stencil underside before expanding slump tests.

02

Separate standard coupons from actual hardware

Material cold and hot slump tests compare contour stability under specified conditions. Fraunhofer's low temperature paste study uses particular specimens and conditions. Its gaps and temperatures are not universal UPS acceptance values. Confirm the method and paste before defining board criteria.

Freeze paste lot, stencil thickness and apertures, environment, printing and waiting time for comparisons. Record hardware position and seating because placement changes local geometry. A coupon without bridges does not qualify the actual hardware and neighboring pad arrangement; one SPI volume check does not cover the entire queue window.

03

Retain matched evidence before changing the process

We recommend a clearly identified principal change per comparison, checking contours, bridges and completed joints at the same locations. Reducing paste also changes solder supply. Recheck wetting, support and required mechanical and electrical performance rather than accepting bridge removal as the sole goal.

Include maximum waiting, pause recovery and material use conditions in the approved process. Reassess changes to paste, apertures, hardware underside or oven program. Touchup appearance cannot qualify the original process. Preserve abnormal boards and records while the cause is unresolved instead of automatically attributing it to the hardware supplier.

04

Frequently asked questions

Can slump occur after an SPI pass? Review subsequent waiting, placement and heating; a single inspection covers its own stage.

Is every reflow bridge hot slump? Check stage evidence and other printing or placement causes.

05

UPS SMT copper hardware RFQ inputs

Provide underside geometry, pads and spacing, stencil and paste information plus stage photographs at the defect. Define supply versus process sampling scope, with geometry checks, cold and hot comparisons and assembly acceptance. Preserve conditions for both good and abnormal specimens.

Apply this guide to a project

Use product pages to identify the hardware family and the calculator for early estimates only. Acceptance depends on drawings, operating conditions and project tests.

Sources

  1. Indium cold and hot solder paste slump influencing factors↗
  2. Fraunhofer ISIT separation of paste contour stability and solder spreading↗
  3. Related industry and selection guidance↗
  4. Submit a drawing and project RFQ↗