A permissible Cu-Al bend radius requires evidence for the specific section, temper and forming route. Define inside radius and copper-side orientation, form representative samples, and inspect dimensions, cracks and the interface. Pure-copper radius tables do not authorize a composite production process.

01

Define the bend on a section drawing

Distinguish inside radius, outside radius and tool radius. Mark copper-layer orientation, total thickness, layer distribution, angle, bend axis relative to the original material, nearby holes and contact faces.

Double-sided, fully clad and local transition structures need separate reviews. Trace specimens to material batch and temper; one successful section does not qualify another layer proportion or joining route.

02

Use a representative forming route

ASTM E290-22's public scope distinguishes bend constraints, radius, angle and measurement before or after unloading. It addresses ductility testing. Composite-product acceptance still requires an agreed specification.

Recommended records include tooling, support spacing, forming passes, speed and lubrication. Unloaded angles and hole positions govern assembly. Repeated corrective bending should be assessed separately if permitted in production.

03

Inspect surface, interface and geometry separately

Examine the outer layer, corners, hole edges and contact regions for cracks, lifting, dents and separation indications. A surface criterion alone does not establish interface integrity; investigate suspected defects using an approved method.

Agree representative interface checks at first-article stage and measure unloaded radius, angle, flatness and hole spacing. If plating or insulation follows forming, final acceptance must include those operations.

  • Lock section, temper, orientation and material batch
  • Retain forming records, unloaded geometry and defect locations
  • Include interface checks and downstream finishes in acceptance
04

Frequently asked questions

Can every part use an inside radius of one thickness? No universal ratio is supplied here; it requires evidence for the selected material and process.

Does a crack-free appearance authorize volume production? Interface, dimensional and final-assembly requirements must also be met using representative conditions.

05

RFQ inputs for formed Cu-Al parts

Supply section and developed drawings, orientation, inside radius, temper, holes, contact faces, insulation scope, quantity and acceptance requirements. If radius remains open, state installation space and adjustment limits so samples can establish a usable process window.

Apply this guide to a project

Use product pages to identify the hardware family and the calculator for early estimates only. Acceptance depends on drawings, operating conditions and project tests.

Sources

  1. ASTM E290-22 public scope of material ductility bend testing↗
  2. CDA and European Copper Institute copper forming guidance↗