Report coating pull-off readings together with failure location. A test glue separating from a dolly answers a different question from insulation detaching from metal. Establish a setup suitable for part rigidity and curvature before discussing acceptance values.
Select a configuration for the substrate
ISO 4624's 2023 edition addresses pull-off methods for paints, varnishes and related coatings, distinguishing rigid and deformable substrate applications. A thin busbar may bend. Instrument capacity alone cannot select the method, and the laboratory must confirm applicability to the insulation system.
We recommend recording conductor thickness, Cu-Al layers, coating system, test locations and support. Identify finished parts versus same-process coupons. A flat coupon does not automatically cover bend interiors, edges and holes with different curvature or thickness.
Include dollies and test glue in the record
Agree dolly size, mating preparation, glue, cure, loading direction and rate, plus whether the coating perimeter is cut. Results with unspecified cutting arrangements should not be ranked by number alone. The laboratory should establish operations under the selected method.
Retain before photographs, coating thickness and conditioning. Resolve poor seating, support effects or glue incompatibility before interpreting the test. Arbitrarily increasing glue thickness to bridge a curved surface does not establish a comparable adhesion strength.
Inspect the fracture after recording the reading
Elcometer distinguishes adhesive separation between layers or substrate, cohesive failure within material and test glue related failure. Retain both fracture faces for each location and report failure type, position and area proportion, with laboratory interpretation of mixed failures.
A test glue failure must not be relabeled as the measured metal to insulation interface strength. If a test stops at an agreed limit without detachment, report that stop condition. Keep coating pull-off, cross-cut classification, Cu-Al interface peel and assembly dielectric tests separate. None supplies an automatic conversion into another result or service life.
Frequently asked questions
Does test glue failure automatically reject the coating? Interpret location and method against agreed criteria first.
Can a pull-off pass remove electrical testing? Adhesion and insulation performance need their respective checks.
Motor controller insulated Cu-Al part RFQ inputs
Provide substrate and coating drawings, thickness, curvature, permitted destructive locations and specifications. Agree specimen preparation, dolly and glue compatibility, individual results, fracture photographs and post-test handling. Define electrical testing separately.
Apply this guide to a project
Use product pages to identify the hardware family and the calculator for early estimates only. Acceptance depends on drawings, operating conditions and project tests.