Compare peel and shear results within their respective test methods. N/mm expresses force per specimen width, while MPa expresses stress per area. They cannot be directly converted into one interchangeable interface-strength rating. Agree the specimen and acceptance basis before comparing supplier reports.

01

Identify the tested object

The cited Cu-Al clad-plate study defines peel specimens, sampling direction and test speed, and calculates peel strength from force divided by specimen width. Its materials and processing conditions belong to that experiment; its results are not acceptance limits for another busbar.

Request a specimen drawing identifying both layers and the loading direction. Keep whole-section tension, interface peeling and joint shear in separate report fields.

02

Record the calculation and extraction rule

For a proposed peel qualification, retain the force curve, specimen width and evaluation interval. State whether the reported value is a mean or a peak. A shear result also needs the area used in its calculation and the actual specimen configuration.

Matching units only aligns notation. Ask the testing party to assess differences in thickness, orientation, gripping and pretreatment. Do not divide a peel result by the complete busbar cross-section to create an apparent shear stress.

03

Keep the failure evidence

Retain images of both fracture surfaces. Distinguish interface separation, parent-metal tearing and grip slip. If the parent metal fails first, record that outcome without assigning an unmeasured exact interface strength.

Use a consistent method for candidate comparison, then link the selected structure to forming, connection and electrical validation. Interface acceptance alone does not establish PCS ampacity or cabinet life.

04

Frequently asked questions

Does a larger peel number guarantee higher shear strength? These loading modes and normalizations require separate evaluation.

Can a paper's test speed be copied into the order? Confirm the applicable method and complete specimen conditions first.

05

ESS PCS busbar RFQ inputs

Provide the layer structure, material condition and finished drawing. Request a specimen drawing, sampling locations, test quantity, raw curves and failure photographs. Have the project team agree acceptance values rather than borrowing a published research result.

Apply this guide to a project

Use product pages to identify the hardware family and the calculator for early estimates only. Acceptance depends on drawings, operating conditions and project tests.

Sources

  1. Cu-Al clad-plate peel specimen and test method research↗
  2. Related industry and selection guidance↗
  3. Submit a drawing and project RFQ↗